Cryogenic Perlite

  • Home
  • Cryogenic Perlite
AttributeValues
Density 45-50kg/m3 (-+%10)
Grain Diameter 0-0,5mm
Sieve Analysis Max. % 10 + 1,18 mm
Min. % 50 + 0,15 mm
Thermal Conductivity Coefficient 0,030-0,040 Kcal/mh C
Chemical Composition Alkaline Oxides
Not effected from oxide and alkaline.
pH= 7 Fusion Temperature 1200 C
Thermal Conductivity in Lower Temperature Value ( - 40 C °) (0,035 - 0.039W / m ° K)
Thermal Conductivity cryogenic materials applications in average temperature value ( - 125 C ° ) (0,025-0,029 W / m ° K)
Package 0,1 m3 Packages

Gallery